Nickel Alloy K500, Monel® K500, UNS N05500, QQ-N-286
STEELMAX Metal Story

 

N05500, Alloy K500 는, Nickel minimum 63%,
Copper nominal 30%, Nickel Copper Alloy금속입니다.

Ni + Cu 합금에 석출 경화 (Precipitation Hardening)
원소인 Ti, Al을 복합 합금한 금속입니다.

내식성 — Corrosion(Erosion) resistance.
고강도 — High strength corrosion fatigue로

비자성 — Non-magnetic
높은 치수 안정성 — Good dimensional stability  성질을 가지며

N04400, Alloy 400 대비
N05500, Alloy K500 이, 약 2배 이상의 높은 항복강도 특성을 가집니다.

UNS Number N05500,또는 K500, Monel® K500, QQ-N-286으로도 불리며
Monel® K 500은 Special Metal Trademark 입니다.

Use for pump shafts, marine propeller shafts, bolting,
impellers, valves components for ships and offshore drilling towers,

doctor blades and scrapers,
electronic components and sensors,

ASTM B865  Specification covers nickel-copper-aluminum alloy
(UNS N05500) in the form of rounds, squares, hexagons or

rectangles and forging and  forging stock, manufactured either
by hot working or cold working, and cold-worked wire.

 

ASTM ASTM B865
UNS No. N05500
Nickel (Ni) 63% min
Copper (Cu) 27~33%
Iron (Fe) 2.0 max
Manganese (Mn) 1.5 max
Carbon (C) 0.18 max
Silicon (Si) 0.50 max
Sulfur (S) 0.010 max
Aluminum (Al) 2.3~3.15
Titanium (Ti) 0.35~0.85

 

 

Form Condition Size Strength (MPa, min.) Elongation Hardness (min.)
Tensile(min.) Yield(min.) (min. %) Brinell 3000 Rockwell C
R, H, Sq, Re, F +H and age-hardened All           965           690             20           265             27
Rounds +C and age-hardened 1/4″<t≤1″         1,000           760             15           300             32
1″<t≤2″           965           690             17           280             29
2″<t≤3″           930           655             20           255             25
Hexagons +C and age-hardened 1/4″<t≤2″           965           690             15           265             27
R, H, Sq, Re, F +A and age-hardened t<1″           895           620             20           250             24
1″≤t           895           585             20           250             24
 R : Rounds, H : Hexagons, Sq : Squares, Re : Rectangles, F : Forging, +H : Hot worked, +C : cold worked

 

 

※ Precipitation Hardening Steels (석출 경화 : 析出硬化)
Steels with the property of being hardened by a method wherein
a small amount of elements such as aluminium, copper, etc.
is added and compounds of those elements or the like are
precipitated by heat treatment.

알루미늄, 구리 등의 원소를 소량 첨가하고, 열처리에 의해
이들 원소 화합물을 석출 시켜 경화 하는 성질을 지니게 한 강.

※ Fatigue Strength (피로 강도 : 疲勞强度)
A property of resistance for breaking to be generated by repeated stress
반복되는 응력으로서 생기는 파괴에 견디는 성질.

※ Corrosion (부식 : 腐蝕)
Physicochemical interaction between a metal and its environment that results
in changes in the properties of the metal, and which may lead to significant
impairment of the function of the metal, or the technical system,
of which these form a part.
This interaction is often an electrochemical nature.

금속과 그 주변 환경의 물리 화학적 상호 작용으로 금속의 성질을
변하게 합니다. 이로 인해 금속, 환경 또는 기술 시스템 전체 또는
일부의 기능에 심각한 손상이 유발될 수 있습니다.
이 상호 작용은 간혹 전기 화학적인 특성을 나타냅니다.

 

20161013_163743

UNS N05500, Ni-Alloy K500, Monel® K500

 

스틸맥스는 연구소 수준의
깊이 있는 철강에 대한 이해를 바탕으로,

Carbon Steel, Special Steel, Stainless, Functional steel,
Ni-Alloy, Cu-Alloy, Al-Alloy, Ti-Alloy, Forging .

Plate, Sections, H-BEAM, Angle, Channel,
Flat, Round Bar, Rail, Pipe & Tube, SMLS,

ASTM, ASME, AISI, ANSI, API, SAE, AS, CSA
EN , KS, JIS, DNV, ABS, GL, LR, KR, NK. RINA, RS, CCA, IACS의

국가규격, 국제단체 규격, 국제협회 규격부터
Mill Maker Standards까지 공급하고 있습니다.

Citius, Altius, Fortius,
더 빠르게, 더 높이, 더 강하게가 요구되는  올림픽처럼

공급이 어려운 철강재 공급에는
진정한 전문 선수를 필요로 합니다.

철강재의 기본 물성치를 바로 확인해 볼 수 있는
스틸맥스(주) 사이트 철강 강종 “500” 바로가기 :
https://steelmax.co.kr/products/plate/


대표적인 철강재의 중량을 자동으로 계산해 주는
철강 중량금액 자동계산기 바로가기 :
https://steelmax.co.kr/calculator/carbon/plate/