EN 10278, Stainless Bright Bar Tolerance, Dimensions
STEELMAX Steel Story
EN 10278 은 허용 공차 규정입니다.
bright bar 에 대한 칫수와 공차 규정으로
공차 규정은 ASTM, DIN EN, JIS, KS 등,
Standard 규정에 각각 있습니다.
EN 10028 의 규정 중 표면에 대한 다듬질의
스테인레스 환봉 (EN 10088-3) 에 대한 규정은 아래와 같습니다.
예를 들어 Stainless steel, DIN-EN 1.4441, 316LVM, ISO 5832-1,
ASTM F138 강재의 경우, Tolerance EN 10278 h9 가, 적용되기도 합니다.
Tolerance class to ISO 286-2 | |||||||
Finished condition | h6 | h7 | h8 | h9 | h10 | h11 | h12 |
Drawn | R | R | R, S, H | R, S, H | |||
Turned | R | R | R | R | |||
Ground | R | R | R | R | R | R | R |
Polished | R | R | R | R | R | R | R |
R = round, S = square, H = Hexagon |
Tolerance class to ISO 286-2 | |||||||
mm | h6 | h7 | h8 | h9 | h10 | h11 | h12 |
>1 to≤3 | 0.006 | 0.010 | 0.014 | 0.025 | 0.040 | 0.060 | 0.100 |
>3 to≤6 | 0.008 | 0.012 | 0.018 | 0.03 | 0.048 | 0.075 | 0.120 |
>6 to≤10 | 0.009 | 0.015 | 0.022 | 0.036 | 0.058 | 0.090 | 0.150 |
>10 to≤18 | 0.011 | 0.018 | 0.027 | 0.043 | 0.070 | 0.110 | 0.180 |
>18 to≤30 | 0.013 | 0.021 | 0.033 | 0.052 | 0.084 | 0.130 | 0.210 |
>30 to≤50 | 0.016 | 0.025 | 0.039 | 0.062 | 0.100 | 0.160 | 0.250 |
>50 to≤80 | 0.019 | 0.030 | 0.046 | 0.074 | 0.120 | 0.190 | 0.300 |
>80 to≤120 | 0.022 | 0.035 | 0.054 | 0.087 | 0.140 | 0.220 | 0.350 |
>120 to≤180 | 0.025 | 0.040 | 0.063 | 0.100 | 0.160 | 0.250 | 0.400 |
>180 to≤200 | 0.029 | 0.046 | 0.072 | 0.115 | 0.185 | 0.290 | 0.460 |
For example a 20 mm nominal diameter having a tolerance class h9 is 20 mm+0, -0.052 mm or 19.948/20. mm |
※ EN 10278 : Standard specification for dimensions and
tolerance of bright steel products
※ Bright Steel : Steel which has had the surface condition improved by drawing, peeling,
turning or grinding the steel finish to produce a “bright” finish with a tighter tolerance
and an improved surface without scale
Cold drawing (Symbol : +C) : increases the yield and tensile strengths,
often eliminating further costly thermal treatments.
Turning (Symbol : +SH) : gets rid of surface imperfections
Grinding (Symbol : +SL) : narrows the original size tolerance range
Polishing(Symbol : +PL) : improves surface finish.
스틸맥스는 연구소 수준의
깊이 있는 철강에 대한 이해를 바탕으로,
Carbon Steel, Special Steel, Stainless, Functional steel,
Ni-Alloy, Cu-Alloy, Al-Alloy, Ti-Alloy, Forging .
Plate, Sections, H-BEAM, Angle, Channel,
Flat, Round Bar, Rail, Pipe & Tube, SMLS,
ASTM, ASME, AISI-AMS, ANSI, API, SAE, AS, CSA
DIN-EN , KS, JIS, DNV, ABS, GL, LR, KR, NK. RINA, RS, CCA, IACS의
국가규격, 국제단체 규격, 국제협회 규격부터
Mill Maker Standards까지 공급하고 있습니다.
Citius, Altius, Fortius,
더 빠르게, 더 높이, 더 강하게가 요구되는올림픽처럼
공급이 어려운 철강재 공급에는
진정한 전문 선수를 필요로 합니다.
철강재의 기본 물성치를 바로 확인해 볼 수 있는
스틸맥스(주) 사이트 철강 강종 “500” 바로가기 : https://steelmax.co.kr/products/plate/
자주 사용하는 대표적인 철강재의 중량과 금액을 자동으로 계산해 주는
철강 중량금액 자동계산기 바로가기 : https://steelmax.co.kr/calculator/carbon/plate/
구매, 문의, 견적, 안내가 필요하신 경우
Contact us 바로가기 : https://steelmax.co.kr/contact/