ASTM A350, Carbon and Low-Alloy for Piping
STEELMAX Steel Story
ASTM A350은 탄소강과 저합금강이면서
Fitting, Valve, Flange 용도의
저온 충격용 Notch 인성 (Toughness)을 중요시한
단조강 ASTM Spec입니다.
A350 은 ASTM 철강재의 Grade, Class 체계와는 다른,
독특한 LF1, LF2, LF3, LF4와 같은
LF 체계를 가지는 강재로 “LF”는 ASTM A350 Standard에
나오는 “Low-alloy steel Forged”의 약자를 의미합니다.
A350 Standard Specification for Carbon and Low-Alloy Steel
Forgings, Required Notch Toughness Testing Piping Components.
A350은 JIS G3205 저온 압력용기용 단강품
SFL : Steel Forging Low Temperature 과 비교 가능하며
JIS G3205 Standard specifies the carbon and alloy steel forgings
imparted a high weldability and to be used for the manufacture
of pressure vessels and other components
for low temperature service 규정입니다.
※ Steels for pressure vessels
Steel products manufactured pressure vessels and high pressure
equipment which require strength, weldability and principally
toughness at a ordinary temperature.
They are generally used for the principal portions of
pressure vessels.
압력 용기 및 고압 설비용으로서 고온 강도, 용접성 및 주로
상온에서의 인성을 중요시하여 제조 된 강재로
보통 압력 용기의 주요 부분에 사용됩니다.
※ Charpy V-Notch Impact Test (CVN)
Test to measure the absorbed energy, impact value, percentage
of brittle/ductile fracture, transition temperature, etc. with using
charpy impact testing machine in which test piece is supported by
two supports distant by 40 mm so that the notch meets the middle
between supports and is broken by striking with one blow of
pendulum to the face opposite the notch.
※ Toughness (인성 : 靭性)
The degree of difficulty in occurring impact breaking
because of the material’s toughness .
질기고 세며, 충격 파괴를 일으키기 어려운지, 어떤지의 정도.
A350 | Grade LF1 and LF5 | Grade LF2 | |
Class 1 | Class 1 and 2 | ||
Chemical composition (%) | Carbon (C) | 0.30 max | 0.30 max |
Silicon (Si) | 0.15~0.30 | 0.15~0.30 | |
Manganese (Mn) | 0.60~1.35 | 0.60~1.35 | |
Phosphorus (P) | 0.035 max | 0.035 max | |
Sulfur (S) | 0.040 max | 0.040 max | |
Nickel (Ni) | 0.40 max | 0.40 max | |
Chromium (Cr) | 0.30 max | 0.30 max | |
Molybdenum (Mo) | 0.12 max | 0.12 max | |
Copper (Cu) | 0.40 max | 0.40 max | |
Cb(Nb) | 0.02 max | 0.02 max | |
Vanadium (V) | 0.08 max | 0.08 max | |
Proof Stress (N/㎟) | 205 min | 250 min | |
Tensile Strength (N/㎟) | 415~585 | 485~655 |
스틸맥스는 연구소 수준의
깊이 있는 철강에 대한 이해를 바탕으로,
Carbon Steel, Special Steel, Stainless, Functional steel,
Ni-Alloy, Cu-Alloy, Al-Alloy, Ti-Alloy, Forging .
Plate, Sections, H-BEAM, Angle, Channel,
Flat, Round Bar, Rail, Pipe & Tube, SMLS,
ASTM, ASME, AISI, ANSI, API, SAE, AS, CSA
EN , KS, JIS, DNV, ABS, GL, LR, KR, NK. RINA, RS, CCA, IACS의
국가규격, 국제단체 규격, 국제협회 규격부터
Mill Maker Standards까지 공급하고 있습니다.
Citius, Altius, Fortius,
더 빠르게, 더 높이, 더 강하게가 요구되는 올림픽처럼
공급이 어려운 철강재 공급에는
진정한 전문 선수를 필요로 합니다.
철강재의 기본 물성치를 바로 확인해 볼 수 있는
스틸맥스(주) 사이트 철강 강종 “500” 바로가기 :
https://steelmax.co.kr/products/plate/
대표적인 철강재의 중량을 자동으로 계산해 주는
철강 중량금액 자동계산기 바로가기 :
https://steelmax.co.kr/calculator/carbon/plate/